I have done several pot metal parts on restorations and not had any problems. They were all stripped of chrome and properly out gassed. The only part that I had to redo was the first one because I didn't outgas long enough and it had a few bumps on it. The first rule I learned was to not get in a rush and do the proper prep.
SS