haha, well initially I got the book from Ron Newman. I used a mix of suggestions between Caswell's suggested and his.

Simply downgrading my tank to a 5gal tank and following the Caswell instructions made the difference. I did loose my connections on all my parts so far after 45min but thats due to me ramping up slightly the amps due to the amps dropping off slightly after time. Again, ill try the suggested 6ASF and not 9 till I get a better rack and more Ti wire. So far, looks like nothing detrmintal has occured from me 1/2 my anodizing time, took the colours and wont rub off (tried after 24h).

Ill check out that wire online store, hopefully they ship to Canada.