I built my booth over the weekend, I will post pics tonight. I haven't had a chance to try it out since my oven quit on me. I used a normal floor vent and duct work and reduced it to fit my shopvac. When I turn on the shop vac it pull air from the booth directly into the shopvac...not sure how well it works since I haven't shot any powder in it yet. I might need to put a small fan or something in it to push more air but we will see. My booth dimensions are quite large but I wanted to contain ALL overspray.

4ft 6in D x 8ft 6in H x 5ft 6in L