the customer came back yesterday whit the pipe
the pc on the heat protector was completely burn and peel off the pipe and the muffler bottom part look like it was muffler
the people at the bike shop did not leave an air gap between the pipe and the heat shield ? for the muffler i guess shooting right over chrome was not a good idea
the customer was in a good mood believe me
so i sandblasted all the parts and sand it whit 180 grit sand paper and shoot it high temp flat black asking him to make sure to leave an air gap between the part and build a custom protector for the bottom of the slip on
something like this ever happened to you, what you think gonna happen next