....ok, I get my parts back from the sandblast guy on friday. I'm ordering my PC Kit today. I will definitely use proper gloves to handle parts. It is best to outgas when my kit arrives, and then shoot hot (150 rule) And this is the technique to do right guys?

pre warm oven to 350
insert part and wait till PART achieves 350 (taken by IR temp gun of course!)
remove to quik clean?(with what?) -then cool to 150 and shoot
enjoy a part in all its gleeming glory!

if I'm missing something point it out guys! Because I'm on my way to being a (trumpets play majestically in the background, champaigne falls from the heavens..pretty girls dance etc..etc..) kick-butt PC'er like you guys!