I checked the label and it says:

MIX WITH 2 GAL DISTILLED WATER, 24 oz battery acid
& the enclosed bottle of brightener

This is for each bag.

If you've flash coppered the part, you don't need to acid copper plate it. Sure, you can use Flash Copper to build up the part.
__________________
--
Mike Caswell
Caswell Inc
http://www.caswellplating.com
Need Support? Visit our online support section at http://support.caswellplating.com
Have A Web Site?
Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm
Reply With Quote