Sswee,

I run all my dye tanks at 140 degrees. Why do you ask?
It was part of Fragglerock's statement; ". . . the dye was at room temp." and
described the dye as "fast blue". I was curious about the temp. control of this dye. I was reviewing his operating parms and
this was one I thought was not in line with Caswell instructions. I have not used this dye myself.

The putters are half polished and half glass beaded.
Actually I did take a good look at your coloring and I liked the results!
The blue is very attractive--- I too have purchased some glass beads to
experiment with coloring results. I bought #12 size which is the finest grade
this particular company sold.
What size glass beads are you using?