Default Re: Anodizing and High Temp Environments

The anodizing should hold up ok, but I don't know whether or not the color would on a long term basis, assuming it was dyed. It will hold up short term, I can say that. I just don't know effects that the extended exposure might have. I would venture to say that the qualities of the dye will be a factor.

A thick anodize, along with an extended seal time and temperature may improve the chances of success.

You may need to do some application testing to find out.