Re: Navy Blue Powder Coat
I know this has come up in the past with mixed opinions, but I just mixed blue and black. I kept adding black until I achieved the color I wanted, which was a navy blue. I passed it multiple times through a sieve, and had no problem with the color being spotted after it was applied and cured. As a matter of fact, I sprayed the navy blue and then applied red on another portion of the part, and ended up with purple where the two colors overlapped. Try it on some test pieces, you've got nothing to loose.
Last edited by blackcamaros; 04-05-2006 at 03:17 PM.
|