i am getting a slightly rough white haze on my nickel plate. it is scattered randomly on the piece. the piece was a polished zincated aluminum part. the manuel suggests it might be excess hydrogen peroxyed in my solution. if this is the case:
1. how does it get in there?
2.how do i remove it?

my solutions are new. there is also some small foreign matter in it . im going to try to filter my solution in hopes of clearing it out of there. what is the best way to filter without haveing to replace any chemicals?