Thread: white haze
View Single Post
  #2 (permalink)  
Old 04-05-2006, 08:15 PM
fly fly is offline
Amateur Metal Finisher
 
Join Date: Jun 2005
Location: beaumont misssissippi
Posts: 310
fly will become famous soon enoughfly will become famous soon enough
Default Re: white haze

Can you give me the exact steps that you took on the part after you did the water test after cleaning.
You can get by without filtering the solution, I don't filter mine and it does good, but filtering is better for the bath..
Make sure you have the correct temp. (140degree) agitation, and correct amps. I will be able to help more with more information.
__________________
www.chrome-plater.blogspot.com
Reply With Quote