can you polish too much?
i repolished some pitted parts of my wheels and it turned out just fine. while inspecting them yesterday it seems like there are a few small parts that appear white. i thought it was left over polish, but i couldn't get it off. it looks like it's underneath the polished metal.
so is it possible to polish too much?
thanks!
|