here are my steps:
degreased
30 sec in pickle #3
zincate for about 1 min
then nickel plate
you wrote 140 for the temp but the manuel says 110 F.
its an odd shaped part but i guess the current could be wrong. i tryed my best to get it as close to exact as i could. here are some pics. hopefully it will help you determine the problem.