Got the kit... Now where do I start!! (Motorcycle frame)
Ok... My winter project (which has turned into a spring project) was to polish the frame on my 2002 Yamaha R6. I tore the bike apart and ordered the "Aluminum wheel finishing & polishing kit) from Caswell. It came yesterday. I used the "anodizing remover" and got that part done. Now what do I do? Use greaseless? The more detailed instructions I could get the better. I really appreciate any help you would be willing to offer. Thanks!