Hey everyone,
I tried that piece of sq tubing, it did not take, I think it was to cold. My buddie's barn is not heated, and it still has not warmed up here yet.
I also have ordered some better dye, can't wait for it to get here!!
I have a couple questions:
1. the manual says that the acid solution is 3 parts water and 1 part acid, is my math off or is this a 25% acid solution?
2. what is the resistor in the electric system for? is this necessary for the system to work?
thanks
Canute
|