Hey everyone,
SS, I am making upgrades to my system while waiting on the dye to arrive, I now have the dimmer switch and some 12 v lights to add to my set up.
In response to your questions:
1. my solution is now 3 parts distilled water and 1 part acid (part=gal)
2. SA of my part is 23.538, according to the 720 rule to get .7 mills, I need 6 amp CD, current set at .98 for 84 mins, with a peak voltage of 15 v

This brings me to a couple of questions:
1.can you explain how to "set" the current, I read about this but I'm not quite sure if I am understanding.
2. The 720 rule says peak voltage is 15 v, I have a 12 v charger, as usual I'm a little short( I'm 5'7" tall) is this a problem?

Also checked with my "tech" and he informs me that rubbing the tub is not an option, this next week temps should be coming up to about 70F, so that should help.