Re: CV anodizing and electrolyte Titration
I'm back now. I'm in the process of locating different alloys. Any help out there? I'm looking for 2024, 6062, 5052, and 7075. Larger samples would be best. I can machine to shape, and pay for shipping.
I got a sweet spread sheat that calculates how much aluminum to add, etc., per titration results.
People, this is advanced stuff here, and contrary to caswells proven methods. If you try CV anodizing, you're on your own. Don't ask for help, don't anodize non-replacable parts, and don't contact caswell with problems. This is just an experiment, and I suspect the results will only confirm the validity of Fibergeeks, and others hard work, which has discovered and proven the LCD method works (and works well).
__________________
Specializing in anodized graphics in Paintball guns.
|