marsfrogie
Send a message via AIM to marsfrogie
Default

Your time will greatly vary depending on wheel size and RPM's.

240grit 2-10 hours
emery 2-6 hours
tripoli 1-3 hours
white 1-6 hours (You may uncover more details such as a small scratch that you missed with the other compounds, white will take them out as long as they don't catch your fingernail.)
That is just a very vague guess. If this is your first polishing job it will probably take you slightly longer to get the hang of it.