Well once you have a nice coat of silva spray you must use acid copper temp should be around 110 but follow the directions in the manual the acid copper should allow you to get the surface you want to be able to plate the copy chrome with out the nickle. Your amps depend on the surfface area of the part you are plating not the amount of solution