Thread: white haze
View Single Post
  #6 (permalink)  
Old 04-11-2006, 12:58 AM
chromepl8tr chromepl8tr is offline
Newbie
 
Join Date: Jun 2005
Posts: 18
chromepl8tr
Default Re: white haze

It appears to may have some old anodizing on it. That is assuming it had any on it in the first place. You may want to gas it in some hot caustic soda for a few minutes and then a nitric acid dip followed by a thorough water rince.
Then polish it all over and replate.