Hi Guys, I am having mixed results with my kit, the last job I did I had the amps up a little higher, and my plate turned out very dark, according to the manual I had "burnt plate" , as it was not decorative I thought I could live with the dark result, but after only 2 days sitting on the bench in the workshop the parts had corroded and rusted very badly. Is this what happens if the plate is "burnt". I am using a lab type power supply with current limiting feature, even when I turn the power supply up full 20 amps and 50 volts ( I know this is far too much) I still do not get any bubbles forming from the part in the bath - which is how the manual tells me to confirm I am using too much power, anyone any ideas why this is no happening, and why my parts rusted almost immediately

On the plus side, I have been getting some excellent results from my nickel plating kit !
Reply With Quote