Default Re: Doing some experiments and need some alloy samples

It would be nice if you could also dip them in the caswell desmut to see if it will remove, on 7075 when you etch and it turns black the caswell desmut will remove every trace of smut, others I'm sure silicon will not do anything.

I have read about other smut removers would be nice to get some of this, but from reading it's a bit nasty

Keep us updated, looks like a sicky in the making, nice clear big images