navel jelly will work, so will 50/50 mix of muratic(hydrochloric acid sold as concrete/pool cleaner) and water. If you want it to be faster, put in a piece of SS sheet or lead, hook the neg side of a battery to it, and the positive side to the part. Keep a close eye on it, it may start removing base metal. Acid can be neutralized with baking soda afterwards.