These were a lot of work. I tried lab metal & JB Weld neither worked well for filling this many pits. The remedy was to fill with the extreme chrome and sand by hand then repeat until you get a smooth surface. When I get caught up later next week I will post a "How To" for doing this. There were several things I learned as I progresed through these pieces.


Yes they are cleared using Jim's instructions found Extreme Chrome with Clear Coat How to...