HI, Thanks for the advice. I guess the word NOT was missing from my post as in the keys are NOT gold or silver- LOL If they were I sure wouldn't be cutting them off Ha ha. Will try the methods you have suggested relating to the compund. Any suggestions on the buffs? I have 2 loaded with red so I will need to replace. They were 1 spiral sewn and 1 muslin. I do need to be able to get into the inner rim of the key to clean and polish.
After I buff I see there is a black greasy residue what is the proper way to remove that and with what? Thanks, I am sure I will have more questions but I am really having fun with this. Elizabeth