Default Re: Dried up compound

Quote:
Originally Posted by crip75
Hello all

I have some greaseless compound I was using . But it now has dried hard in the bag ?? Is it useless now?
How are you suppose too store this stuff once its open ?
Thanks for the help.

Ed
When I get a new tube of greaseless, I rubber-band a baggie over the end. When it's down to where it'll fit into a Pringle's can, I wad up a wet paper towel, put it in the can and put the tube in, open end down. Put the lid on the can.

You might be able to get some use out of that dry tube by soaking the end in water - try it for a half hour at first. You still might have to really jam it on a running wheel to get any out of it, but might be worth a try.

Last edited by mpierich; 04-17-2006 at 05:45 PM.