Thread
:
Low temp powders?
View Single Post
#
3
(
permalink
)
04-17-2006, 10:43 PM
speedyshark
Newbie
Join Date: Mar 2006
Posts: 9
Re: Low temp powders?
I was going to coat the plastic with copper powder do you think that will crack? If it is calling for 10 min@400 I guess it will not work to put it at lower temp for longer time.
speedyshark
View Public Profile
Send a private message to speedyshark
Find all posts by speedyshark