Default Re: Low Voltage

I have come to the point where I mainly steam seal everything. 90% of parts will seal perfect when dipped in boiling water, it's the 10% that leaches dye all the way from the pores that is the problem. Most of the dye leaching from whati have seen is from cast aluminum, still it seems to work better for me to just steam seal everything, and then spray it down with wd40 I think it was acidraing who gave me the idea on wd40, it works

Clint