It's all about SFPM:

For best results your wheel should maintain a surface speed of between 3600 & 7500 Surface Feet Per Minute. (SFPM). The higher your speed, the better and quicker your results.

Formula for calculating surface speed of wheel in SFPM.

SFPM = 1/4 x diameter of Wheel x RPM (revs of spindle per min.)

Therefore an 8" wheel @ 3600 RPM =2 x 3600 = 7200SFPM.

However, your drill may not be able to spin 6" or 8" wheels because it may not have enough power. If you can press a wheel against the part you're buffing without stopping the motor, you're safe.
__________________
--
Mike Caswell
Caswell Inc
http://www.caswellplating.com
Need Support? Visit our online support section at http://support.caswellplating.com
Have A Web Site?
Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm
Reply With Quote