Quote:
Originally Posted by rick201
Why do you use wd40 after the sealing treatment what are the benefits i may have to try it.
Does it make a better finish and do you soak it or spray on and buff off etc ?
Best Regards to all
Richard..
I use it after the piece is sealed to restore oil to the part, the part should be void of all oils, this will even colors out and give a more natural look after the part is sealed, I think it also serves to do some type of protection, and I use steam to seal, the wd40 will remove any left over dye