Hello,
We have a brushed, stainless steel refrigerator that has some discoloring from an adhesive (pics 1 and 2), along with some surface scratches (visible in all pics - see web link below). I have tried barkeepers friend, stainless steel magic, and hopes silver polish to polish out the scratches and stains, but they do not seem to work. They actually seem to scratch it a little more, and take off a coating that leaves a black residue on the cloth I am using. So, I was wondering if there is really anything I can do to make it look better? For instance, will the green stainless steel compound and a spiral sewn wheel mounted on a portable drill work? Any ideas

Thanks,
Royce
http://www.geocities.com/royceandkri...?1049299216400