After I applied the copper-plate, I stored the items in a sealed tupperware container. Would the fact that the items were in contact with each other be a factor? (Hmmmmmm. Let me guess that the answer will be......."Yes.")
So, in the future, I should immediately plate the gold over the copper?
Thanks!
Mike
|