Default Re: Low Voltage

Hi SS,

One of my problems is too much information from too many different sources. Reading too many articles before starting and adding information from one to another. Somewhere I read that someone was checking acid bath with battery hydrometer and setting acid concentration at 1100. Turns out to be about 1 – 1.

I though “Heck” I’ve got some battery acid, battery charger and battery hydrometer out in shop, I can try this. Got some Rite dye and tried it and got OK results.

That’s how I got going on a 1 -1 acid concentration. I have a small three gallon tank, so will be no big deal for me to reset acid concentration. Will end up with larger acid bath. That may be a plus. Kind of like horsepower If some is good, more is better and way too much is just right.

Thanks for the help. Jim