View Single Post
  #5 (permalink)  
Old 04-20-2006, 02:00 PM
speedyshark speedyshark is offline
Newbie
 
Join Date: Mar 2006
Posts: 9
speedyshark is on a distinguished road
Default Re: powder that cures at 250f

Hey who makes the 150f? What I am going to try is spray part with high temp clear and then dust with copper powder. I think it will work. If it works it will not be much more to powder plastic that it is to do metal. Like you said can only get low temp in large orders. would be nice if caswell would get it and sale small amounts.
Reply With Quote