Just made 40 Titanium spring wire clips
View Single Post
#
4
(
permalink
)
04-20-2006, 11:34 PM
rclint
Amateur Metal Finisher
Join Date: Aug 2005
Posts: 116
Re: Just made 40 Titanium spring wire clips
Here is a picture, hard to get the wire to show up well, white piece of paper seems to work