Default bright nickel problems

I came upon some problems with my nickel bath.It started out with a roughness on the top of parts,now it has turned into tiny pits all over.I have carbon filtered for 10 hrs while dummy plating,then added some brightener and wetter,still have the problem,but now I also have some blisters to go along with it.please help!!!!!