O.K. SS, I got my power supply, ran my 1st test part, came out great!!
So now I'm feeling cocky and I want to try to do 2 colors(splash), I was wondering about the rubber cement, how clean of a line will it give, is there something that will give clean lines and come off easy?
Also,just so I am clear, you ano, then mask, let dry, then dye(darker colors 1st), then strip off the mask, and dye the next section(lighter color), is this right? All advice is welcome.