Re: green and blue dye probs
No, the fish tank heaters don't get hot enough. The cheap and easy is either Caswell 300W heater and thermostat (best) or a large stainless stew pot from the dollar store and a cheap hot plate (will work). The low setting on most hot plates is around 140*.
SS
Last edited by sswee; 04-22-2006 at 06:15 PM.
|