Default Re: Masking questions

1.anno
2.dye
3.mask
4.let mask dry good (unless sticker)
5.dip in bleach
6.rinse good with distilled water
7.Dip in acid (like acidrain said)
8.Wash again very good with distilled water
9.dye 2nd color
10.seal for a short time
11.remove mask
12.seal for rest of time
13.Spray with WD-40

I was thinking maybe run the part for 5 minutes or so after it has been masked and bleached to help the ano layer alittle more...Im not the best in this subject yet though....and will rubber cement dry under water?