Re: green and blue dye probs
I have been doing a lot of small parts, so I use the rubber made small food stoarge containers (cheap 4 packs like you tak eto work and eat out of) I nuke them in the microwave till I get 140*. It takes about 3 minutes on most of them, I also have some larger ones that may take 6 minutes
Saves a lot of time and power compared to other heating methods, not messy, and so far I have not seen any harm to the dye using the nuker
Clint
|