Going to have a 75 gallon rectangular tank inside a 140 gallon rectangular tank with ice water circulating around it. I have tried several methods and feel this is the best - works out to almost the same ratio of water to cool the anodizing. Also going with circulating pump for the acid to keep heat off parts.