Thumbs up Re: Dried up compound

Quote:
Originally Posted by crip75
Well thanks for the help guys. I put it in a plastic bag with a bit of water and, it softened up again. Tried it yesterday and it works fine. Thanks again.
That's great! BTW, my wife does let me use the crisper in the fridge for spares, but I wrap them up real good...