More Ceramic Coating ?'s
I was wondering since ceramic coating cures at 500* for one hour, since my oven goes to 485*, is it just like powder and maybe add say 20 minutes or more cook time and it will fully cure? One other thing...say I ceramic coated an intake manifold, then afterwards I powder coated it. Will the powder adhere to it or separate?
|