Hey acidrain, this is great, I just ran a part that came out of ecthing with a kind of dark gray-greenish-black film on it, since I don't have any de-smut, I just wiped them off and ran them, they came out a little lighter than I had hoped.
Thanks for sharing this info
Canute
|