Quote:
Originally Posted by
princessprofile
"Orange Peel " can also be a sign of over polish...
and that is my 1st 2 cents
Thanks. Wasn't exactly orangepeel, but who knows.
If I had the energy I'd take a few metallurgy courses....
mpierich