I have not thickened the bleach, just let it run on very wet with a low bleach concentration. I think I had mine two strong. Some have suggested a 5:1 ratio Water:bleach.

I watch it pull the dye out of the annodonic layer, and then spray off with my distilled water quickly. it takes some time and patience, and i need to play more but I am really excited about it.