I would imagine that the part and the powder are going to be the same temperature in the oven. Afterall, how could they be different temps when they are both in the oven?
Not so! The powder coated part is not going to be the same temperature, as the oven, until it reaches the curing temperature after it is put in the oven. Also if you 'hot flock' a part, the powder will not instantly reach the temperature of the part, until it is returned to the oven to cure.