View Single Post
  #10 (permalink)  
Old 04-26-2006, 07:02 PM
acidrain acidrain is offline
Metal Finishing Guru
 
Join Date: Sep 2004
Posts: 889
acidrain is on a distinguished road
Default Re: First experiments... Smut pics identify alloys, voltage curves at 6A CD

Blackcote, I have not run at different temps, because I REALLY make an effort to control the temp very precisely. I learned early on that tank temps are one of the first variables that need to be controlled if you want to have consistant results (to the point of desilution after 70F).
I can tell you the difference between 70F, and 68F, is about .5v higher (for a cooler tank).
__________________
Specializing in anodized graphics in Paintball guns.
Reply With Quote