Thread: is it me or?
View Single Post
  #2 (permalink)  
Old 04-26-2006, 08:03 PM
jtagger19 jtagger19 is offline
Experienced Metal Finisher
 
Join Date: Apr 2004
Posts: 466
jtagger19 is on a distinguished road
Default Re: is it me or?

gold , orange, yellow , brass and some coopers almost never reach the desired colors unless used over real chrome or polish surfaces
if they are used over chrome powder they loose it's colors deeps
for the spots in the pictures that is a coating problem noting to do with the color
it could have been a Ground problem.

Last edited by jtagger19; 04-26-2006 at 08:05 PM.