Originally Posted by jtagger19
gold , orange, yellow , brass and some coopers almost never reach the desired colors unless used over real chrome or polish surfaces
if they are used over chrome powder they loose it's colors deeps
for the spots in the pictures that is a coating problem noting to do with the color
it could have been a Ground problem.
Thanks for the reply but after talking with someone from caswell on the phone I found out that the chrome needed to bake longer than what was called for. Since it didnt the orange and chrome tried to blend together creating this color. They are sending me some replacement powder. As for the colors mentioned above I think your partially wrong. I have had many colors come out perfect. Maybe its luck on my part..